Cyclic Corrosion Test (CCT)

Cyclic Corrosion Test (CCT)

For most artifical accelerated tests in laboratory, getting a consistent testing results with outdoor is the most important purpose. Prior to cyclic corrosion testing, conventional salt spray (a continuous salt spray at 35˚C), was the most popular way to simulate corrosion in a lab. Because conventional salt spray methods failed to simulate the natural wet/dry cycles of the outdoors, test results frequently provided poor correlation to outdoors.

Model BGD 886/T BGD 887/T BGD 888/T
Working Room Size (WxHxD in mm) 1200x800x1000 1600x800x1000 2000x800x1200
Working Room Capacity (excluding V-shape cover) 960L 1280L 1920L
Overall Size (mm) 2500x1650x1220 2900x1650x1220 3300x1720x1420

 